Effect of thermo-mechanical load cycling on silorane-based composite restorations (2012)
Source: Dental Materials Journal. Unidade: FOB
Subjects: CARGA TÉRMICA, RESINAS COMPOSTAS, RESTAURAÇÃO DENTÁRIA
A citação é gerada automaticamente e pode não estar totalmente de acordo com as normas
ABNT
BORGES, Ana Flávia Sanches et al. Effect of thermo-mechanical load cycling on silorane-based composite restorations. Dental Materials Journal, v. 31, n. 6, p. 1054-1059, 2012Tradução . . Disponível em: https://doi.org/10.4012/dmj.2012-105. Acesso em: 03 jun. 2024.APA
Borges, A. F. S., Santos, J. de S., Ramos, C. M., Ishikiriama, S. K., & Shinohara, M. S. (2012). Effect of thermo-mechanical load cycling on silorane-based composite restorations. Dental Materials Journal, 31( 6), 1054-1059. doi:10.4012/dmj.2012-105NLM
Borges AFS, Santos J de S, Ramos CM, Ishikiriama SK, Shinohara MS. Effect of thermo-mechanical load cycling on silorane-based composite restorations [Internet]. Dental Materials Journal. 2012 ; 31( 6): 1054-1059.[citado 2024 jun. 03 ] Available from: https://doi.org/10.4012/dmj.2012-105Vancouver
Borges AFS, Santos J de S, Ramos CM, Ishikiriama SK, Shinohara MS. Effect of thermo-mechanical load cycling on silorane-based composite restorations [Internet]. Dental Materials Journal. 2012 ; 31( 6): 1054-1059.[citado 2024 jun. 03 ] Available from: https://doi.org/10.4012/dmj.2012-105